Decide on geometry, wall thickness and order volume. Wet moulded fibre suits thin-wall, shallow, high-volume parts — clamshells, lids, trays — with flat surfaces, cheap tooling and fast changeover. Dry thermal pressing suits thick-wall, deep-draw or structural parts such as cutlery and industrial inserts, with higher density and dimensional accuracy but steel tooling and a slower cycle.
Wet route: slurry forms on a wire tool, then dries and is pressed. Tooling is cheap, changeover is quick, 1–3 mm walls are comfortable. Deep draws suffer uneven wall distribution and corner cracking, and drying is the heaviest energy line in the cost model.
Dry route: compounded fibre is pressed in a heated steel tool. Density, dimensional stability and features such as threads and snap fits are achievable. Tooling cost is an order of magnitude above a wire tool, cycle time is slower, and thick sections can cure unevenly at the core.
Hybrid: form wet, then calibrate in a heated tool. Good for export programmes that are fussy about both surface and dimensions. Longer process chain, friendlier yield.
Run three numbers before committing: tooling amortisation (volume ÷ tool cost), energy per piece, and rework cost on rejects. Short runs and many SKUs favour wet; long runs with structural requirements favour dry. Cutting steel without those three numbers is the most common way money is lost in this category.
| Wet moulded fibre | Thin wall / shallow / high volume; cheap wire tooling, fast changeover, energy-intensive drying |
|---|---|
| Dry thermal pressing | Thick wall / deep draw / structural; expensive steel tooling, slower cycle, tighter tolerance |
| Hybrid | Wet forming plus heated calibration — surface and dimension together |