It runs on conventional lines, with two adjustments: corona treatment to lift surface energy above 38 dyn/cm, and lower seal temperature and pressure to suit the filler level. Bamboo flour is a rigid particle that interrupts resin continuity across the seal interface, so seal strength falls as loading rises. A co-extruded pure-resin sealing layer is the usual fix.
Surface energy: filled film generally sits below plain PE. Untreated, ink adhesion is poor and laminates delaminate. Corona is the cheapest fix but decays with time — convert within about two weeks, or verify with dyne pens before printing.
Sealing: filled systems have low melt strength and a narrow window. Too hot and the seal embrittles and strings; too cold and you get a false seal that looks fine and fails on drop test. Build a seal curve per formulation and run in the middle of the strength plateau, not at its edge.
Printing: surface printing works, but register accuracy tracks web flatness; reverse printing needs lamination, and filler particles cause pinholes. Most export programmes go for few colours and large blocks — lower risk, and consistent with the current direction on material reduction.
Hard constraint: if the roll is to be claimed compostable, inks, adhesives and the sealing layer all fall inside the EN 13432 assessment. Standard solvent-based inks will fail the whole roll. Specify from the finished roll backwards, not from the substrate forwards.
| Surface treatment | Corona to ≥ 38 dyn/cm, used within about two weeks |
|---|---|
| Sealing | Lower temperature and pressure by filler level; run mid-plateau |
| Structure | Co-extruded pure-resin sealing layer for seal strength |
| Certification boundary | Inks, adhesives and sealing layer all inside the EN 13432 scope |